The cold ramming carbon materials stipulate the classification and technical requirements for the cold carbon materials used in the blast furnace and the aluminum electrolysis tank.
Classification: cold carbon materials are divided into two varieties and five brands. 1. the cold tamping material for the blast furnace (1).HT-1 is suitable for the joints between the bottom of the furnace and the filling of the carbon block or the small blast furnace lining. (2).HT-2 is suitable for the gap between the lining of the blast furnace and the cooling wall (or the shell). 3) HT-3 is suitable for blast furnace iron mouth and sand mouth. 2. Cold ramming carbon material ( 1 ) HT-1 for aluminum electrolytic cell is suitable for the joint between aluminum electrolytic cell cushion and filling carbon block or small electrolytic cell lining
Model Index | HT-1 | HT-2 | HT-3 | HT-1 | HT-2 |
Volatiles% | <11 | <12 | <10 | <12 | <10 |
Ash Content% | ≤12 | ≤12 | ≤12 | ≤12 | ≤10 |
Water Content % | ≤1 | ≤1 | ≤1 | ≤1 | ≤1 |
Fixed Carbon% | ≥76 | ≥76 | ≥77 | ≥76 | ≥77 |
Construction Temperature % | 25-40 | 20-25 | 45-55 | 25-40 | 40-50 |
Maximum Granularity% | ≤8 | ≤8 | ≤10 | ≤8 | ≤2 |
After Forming Bulk Density g/cm ³ | ≥1.5 | ≥1.5 | ≥1.5 | ≥1.55 | ≥1.6 |
Compression Strength1300ºCafter burningMPa | ≥25 | ≥20 | ≥25 | ≥25 | ≥20 |
Apparent Porosity1300ºCafter burning% | ≤22 | ≤24 | ≤22 | ≤22 | ≤22 |
Resistivity 1300ºCafter burningΩm | - | - | - | ≤70 | ≤65 |
Breakage Coefficient | - | - | - | ≤1.0 | - |
Purposes | Small blast furnace lining for the bottom layer of the blast furnace and the filling of carbon block | Used for cooling lining of inner wall of blast furnace | For blast furnace tapping and skimming ports | For aluminum electrolytic cell cushion and filling carbon block joint or small electrolytic cell lining | The joint of the swallowtail slot for the cathode of a aluminum electrolytic cell |
FAQ
1.Can you provide free sample?
Yes, we can. But we are not responsible for freight.
2.Delivery Time?
After placing the order, Delivery time will be 18-25 days after the payment is done.
3. Payment Terms
T/T, L/C
4.Why do you choose us?
√ Our factory is located in the industrial area.
√ Our manager is a technician about refractory material.
√ We enjoyed good reputation among our clients.
√ If you have needs, please feel free to contact us